⺠The maximum shrinkage rate of SDC was about 0.4% of that of SDC2. ⺠Three regions could be divided during SDC2 sintering. ⺠The activation energy of SDC2 was 5.54 ± 0.50 eV because of a liquid phase in grain boundary. ⺠The grain boundary diffusion dominant densification with 4.2 Ã 10â17 m3 Nâ1 sâ1 at 900 °C. ⺠The OCV of the cell using SDC2 as electrolyte is 0.78 V at 600 °C.