7743771 Journal of Power Sources 2012 8 Pages PDF
Abstract
► Two freezing types at cold start in and on the surface of a cathode catalyst layer. ► Direct observation of the ice formed on the catalyst layer surface. ► Temporary performance deterioration at 30 °C caused by ice on the surface.