Article ID Journal Published Year Pages File Type
9760536 Journal of Power Sources 2005 10 Pages PDF
Abstract
In high temperature electrical generators such as thermal batteries, the molten salt electrolyte needs to be retained by a binder, e.g. MgO. We have pointed out that the magnesia volume fraction was a more accurate parameter than the usually used weight fraction. Moreover, based on our technique measurements, we defined a magnesia volume fraction range (27-30 vol.%) where the electrolyte retention could be considered as efficient whatever its nature. And finally, we proposed a microstructure description of the retained electrolyte.