4298360 | 1288351 | 2012 | 4 صفحه PDF | دانلود رایگان |
ObjectiveTo test the tensile properties of knotted suture made of 4 different suture materials and exposed to petroleum gauze.Study DesignWe tested the tensile strength of United States Pharmacopeia size 0–0 gauge polydioxanone, polyglyconate, glycolide/lactide copolymer, and silk when exposed to petroleum packing or saline. Suture materials were randomized, and knots were tied and then evaluated via tensiometer to the point of knot failure.ResultsA total of 285 knots were tied in 8 groups based on material and exposure to saline or petroleum gauze. We found that petroleum exposure knots failed at a mean of 116.7 N (SD = 31.5) and that saline soaked knots failed at 123.8 N (SD = 32.0). We conducted a 4 × 2 factorial analysis of variance, finding knots exposed to petroleum failed at a statistically significantly lower tensile strengths than saline soaked knots (p = 0.002).ConclusionPetroleum-exposed sutures fail at lower tensions than saline-exposed sutures.
Journal: Journal of Surgical Education - Volume 69, Issue 1, January–February 2012, Pages 37–40