Bound rubber formation was investigated in detail by applying various extraction temperatures (at room temperature, 90°C, and 180°C) and novel treatment methods (ammonia bubbling and sonication). Bound rubbers could be divided into three major components of core shell, primary layer including tightly primary layer and occluded rubber, and secondary layer including connecting filament. Bound rubber content of the core shell was measured by four successive procedures of extraction at room temperature, ammonia bubbling, extraction at 180°C and sonication. Bound rubber content of the tightly primary layer was measured by three successive procedures of extraction at 90°C, ammonia bubbling and sonication. Bound rubber content of the primary layer was measured by two successive procedures of extraction at 90°C and sonication.
Journal: Polymer Testing - Volume 40, December 2014, Pages 170-177