Comparative Performance of Uranium Bioleaching from Low Grade Indian Apatite Rock in Column and Bioreactor
موضوعات مرتبط
مهندسی و علوم پایه مهندسی انرژی انرژی (عمومی)
پیش نمایش صفحه اول مقاله
Comparative Performance of Uranium Bioleaching from Low Grade Indian Apatite Rock in Column and Bioreactor
چکیده انگلیسی

Uranium ore from the Narwapahar mines, Jharkhand, India (∼0.047% U3O8), rich in apatite content (5%) was investigated for bio-processing in lab-scale columns and bioreactor. With a load of 2.0 kg ore in column at pH 1.7 using A. ferrooxidans and L. ferrooxidans, uranium recovery of 57% and 66% was achieved, respectively in 40 days in comparison to 39% in chemical leaching. Bio-leaching studies with the Narwapahar ore carried out in a 2L bioreactor at 10% (w/v) pulp density at pH 2.0, rpm 150 and 35oC yielded 57% and 63% uranium recovery by 10% (v/v) enriched culture of A. ferrooxidans and L. ferrooxidans, respectively in 5 days. In another set of experiments, biogenic ferric sulfate generated in the bioreactor was mixed with the ore slurry and 90.3% uranium biorecovery was achieved in 10 h at pH 2.0, 20% (w/v) pulp density of <45 μm particles and 40oC with L. ferrooxidans as against 87% leaching at 35oC with A. ferrooxidans.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Energy Procedia - Volume 39, 2013, Pages 20-32