Full length articleWear resistance of machine tools' bionic linear rolling guides by laser cladding
ترجمه فارسی عنوان
مقاله کامل طول مقاومت خطوط نورد خطی بیونیک ماشین آلات با پوشش لایه
کلمات کلیدی
مقاومت در برابر سایش رول، راهنمایی خطی بیونیک، روکش فلزی لیزری،
موضوعات مرتبط
مهندسی و علوم پایه سایر رشته های مهندسی مهندسی برق و الکترونیک
چکیده انگلیسی


- Samples with bionic units present better rolling wear resistance than the untreated.
- The reticulate sample with unit space 3 mm possesses the least mass loss, a reduction of 86.38%.
- The samples with ratio value between 0.15 and 0.3 present better wear resistance.
- The samples with striate shape perform better wear resistance than the other shape groups on the whole.

In order to improve the rolling wear resistance (RWR) of linear rolling guides (LRG) as well as prolong the life of machine tools, various shape samples with different units spaces ranged from 1 to 5 mm are designed through the observation of animals in the desert and manufactured by laser cladding. Wear resistance tests reproducing closely the real operational condition are conducted by using a homemade linear reciprocating wear test machine, and wear resistance is evaluated by means of weight loss measurement. Results indicate that the samples with bionic units have better RWR than the untreated one, of which the reticulate treated sample with unit space 3 mm present the best RWR. More specifically, among the punctuate treated samples, the mass loss increases with the increase of unit space; among the striate treated samples, the mass loss changes slightly with the increase of unit space, attaining a minimum at the unit space of 4 mm; among the reticulate treated samples, with the increase of unit space, the mass loss initially decreases, but turns to increase after reaching a minimum at the unit space of 3 mm. Additionally, the samples with striate shape perform better wear resistance than the other shape groups on the whole. From the ratio value of laser treated area to contacted area perspective, that the samples with ratio value between 0.15 and 0.3 possess better wear resistance is concluded.