چکیده انگلیسی
It was found that the hardness of the hypereutectic coating was significantly higher than the hypoeutectic coating. In both cases, optimum hardness was achieved within the first deposited layer. The abrasion tests showed that there was no significance difference in the wear resistance of the hardfacings at the higher loads and there was contrasting wear behaviour in the dry and slurry conditions. The abrasive wear mechanisms were found to be predominantly microploughing and microcracking in the hypoeutectic and hypereutectic coatings, respectively.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Wear - Volume 263, Issues 1â6, 10 September 2007, Pages 99-110
Journal: Wear - Volume 263, Issues 1â6, 10 September 2007, Pages 99-110
نویسندگان
V.E. Buchanan, P.H. Shipway, D.G. McCartney,