Monodisperse nonporous silica particles were prepared by sol-precipitation via seed particle growth method, and the particle size, which varied from 1.0 to 4.7 μm, was strictly controlled in our experiment. The formation of secondary particles, which resulted in a multimodal distribution of particle size, was suppressed by changing tetraethoxysilane (TEOS) concentration and reaction temperature. Furthermore, the effect of adding small amounts of electrolyte to the hydrolysis mixture was examined.
Formation of secondary particles was suppressed by changing TEOS concentration and reaction temperature, so that monodisperse nonporous silica particles were prepared with particle size controlled up to 1.0–4.7 μm.Figure optionsDownload as PowerPoint slide