On the re-characterisation of defects in structural integrity assessments due to snap-through
چکیده انگلیسی
In TAGSI's view re-characterisation needs to be considered separately for contained plastic collapse and ductile or brittle fracture of the remaining ligament. For plastic collapse and ductile tearing of the remaining ligament the R6 rules for re-characterisation appear generally satisfactory. For brittle failure of the ligament in many cases the R6 recommendations will be found satisfactory but for cases of large difference between static and dynamic toughness it is recommended that scoping calculations should be carried out for the defect geometry, loading and material properties of concern.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Pressure Vessels and Piping - Volume 83, Issue 8, August 2006, Pages 618-623
نویسندگان
, ,