کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
792880 1466744 2015 6 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Characterization, shear strength and corrosion resistance of self joining AISI 304 using a Ni Fe–Cr–Si metallic glass foil
موضوعات مرتبط
مهندسی و علوم پایه سایر رشته های مهندسی مهندسی صنعتی و تولید
پیش نمایش صفحه اول مقاله
Characterization, shear strength and corrosion resistance of self joining AISI 304 using a Ni Fe–Cr–Si metallic glass foil
چکیده انگلیسی

This work studied the microstructure of the interlayer formed after self joining of AISI 304 stainless steel, using a commercial metallic glass foil as the joining element and its effect on the shear and corrosion resistances at the interface zone. Different joining times and temperatures were used varying from 25 to 90 min, and 800 °C, 900 °C and 1000 °C, respectively. The joining process induced an inter-diffusion of alloy elements from the steel to the amorphous foil, conveying to the formation of intermetallics and second phases at the joining interphase, as was observed by SEM. The residual porosity at the joining zone was reduced as both, the bonding time and temperature increased. The mechanical behavior of the bonded samples was evaluated by shear tests presenting a maximum value of 108 MPa for joints produced at 900 °C for 60 min, however the shear test presented values higher that 75 MPa for the temperature vary from 850 °C to 1000 °C and time of 45 min. Fractures occurred on the interlayer, indicating a strong relationship between the microstructure of the interface and the mechanical strength of the joints. Electrochemical tests in 3.5 wt.% NaCl solution presented pitting corrosion at room temperature under conditions of open circuit potential in the form of preferential dissolution.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Materials Processing Technology - Volume 223, September 2015, Pages 16–21
نویسندگان
, , , ,