Tribological behavior of Cr2O3 coatings as bearing materials
چکیده انگلیسی

In this study, the tribological behavior of Cr2O3/Ni8.5Cr7Al5Mo2Si2B2FeTiO2 coatings for bearing materials was investigated in dry and acid conditions. Flame spray technique was used in order to deposit coating materials onto AISI 304L steel substrate. The coated samples were characterized by means of an optical microscope, scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), surface roughness and microhardness testers. The wear experiments were performed under dry and acid environments using a pin-on-plate configuration against AISI 303 counter material for different loads. It was found that in acid environment, the amount of wear loss is less than that of in dry condition and applied load level is more effective in dry condition. In SEM study, the effect of plastic deformation of adherent and compacted debris particles on friction of the coatings was investigated.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Materials Processing Technology - Volume 196, Issues 1–3, 21 January 2008, Pages 259–265
نویسندگان
, , ,