کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
818884 | 906538 | 2013 | 7 صفحه PDF | دانلود رایگان |
Blend of polybutadiene (BR) rubber with varying ratios of chlorosulphonated polyethylene rubber (CSM), BR/CSM, keeping the total waste rubber powder (WRP) content constant at 50 phr (parts per 100 rubber) have been prepared on a laboratory-size (300 × 600 mm) two-roll mixing mill maintained at 40 ± 5 °C. The mechanical properties, namely tensile strength (TS), tensile modulus at 100% elongation (M100), elongation at break (Eb%) and hardness have been followed up as a function of irradiation dose (dose rate of 10 kGy h−1 and total absorbed dose of 100, 200, 300 and 400 kGy) as well as blend composition. The results indicated that the addition of CSM has improved the properties of BR/CSM rubber blends waste rubber powder filled composites. The improvement in mechanical properties of the BR/CSM/WRP (50/50/50) rubber blends is in correlation with homogenous WRP distribution which has been assigned by scanning electron microscopy. Also BR/CSM rubber blends waste rubber powder filled composites are thermally and irradiation more stable than BR and CSM rubbers alone.
Journal: Composites Part B: Engineering - Volume 45, Issue 1, February 2013, Pages 178–184