The aim of the study was to investigate the effects of thermal treatment on the mechanical and physical properties of wild pear wood. The results obtained for thermal treatment at 160 °C for 2 h showed that the modulus of elasticity was increased about 5%, while bending strength and compression strength decreased by 7.42% and 7.55%, respectively. The physical properties of wild pear wood were improved as 2.6%, 5.3%, 8.5% and 0.8% swelling in tangential, radial and longitudinal sections and 1.7%, 1.1% and 0.9% at 50, 65 and 85 Rh% and changes in ΔEab∗ was 8.50%, respectively. It was determined that the changes ratio of these properties increased as the temperature and durations were increasing. Therefore, wild pear wood can be used as an alternative for tropical woods in decoration and veneer industry.