Tensile behaviours of quartz, aramid and glass filaments after NaCl treatment
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
سایر رشته های مهندسی
مهندسی (عمومی)
پیش نمایش صفحه اول مقاله
چکیده انگلیسی
Quartz, aramid and glass filaments were treated with NaCl solutions of various concentrations for different periods of time. The appearance of the treated filaments was examined. It revealed that for the quartz fibre the NaCl density and the treatment time have a minor effect as far as the decrease rate of the fibre strength is concerned. After three weeks of NaCl treatment, dramatic degradation of the aramid filaments was noticed for all the NaCl densities used in the investigation. The glass fibre degradation induced by the NaCl solution was considered regular; both higher NaCl concentration and prolonged treating time would both promote the decrease of the fibre strength.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials & Design - Volume 30, Issue 3, March 2009, Pages 867–870
Journal: Materials & Design - Volume 30, Issue 3, March 2009, Pages 867–870
نویسندگان
Huang Gu,