Cold Deep Drawing of Commercial Magnesium Alloy Sheets
موضوعات مرتبط
مهندسی و علوم پایه سایر رشته های مهندسی مهندسی صنعتی و تولید
پیش نمایش صفحه اول مقاله
Cold Deep Drawing of Commercial Magnesium Alloy Sheets
چکیده انگلیسی
A cold deep drawing process for commercial AZ31 magnesium alloy sheets was developed. The commercial sheets were successfully formed into circular cups at room temperature by optimising the annealing temperature of the sheets, i.e. a limiting drawing ratio of 1.75 was attained for an annealing temperature of 500 °C. The increases in elongation, n-value and r-value, and the decrease in flow stress effective in the improvement of drawability were obtained for the annealing. The apparatus for cold deep drawing without heating becomes much simpler than that for the conventional warm deep drawing. The effects of the lubricant, the clearance between the die and the punch and the corner radius of the punch on the drawability were examined. The limiting drawing ratio was increased by applying force onto the edge of a blank through the die corner. In addition, cold deep drawing of magnesium alloy square cups was performed. It was found that comparatively shallow magnesium alloy cups are satisfactorily formed at room temperature without heating.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: CIRP Annals - Volume 56, Issue 1, 2007, Pages 285-288