کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1251218 970895 2007 4 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Preparation of Crack-free 3Y-TZP/AI2O3 Composite Ceramic Fiber by Electrolysis-sol-gel Method*
موضوعات مرتبط
مهندسی و علوم پایه شیمی شیمی (عمومی)
پیش نمایش صفحه اول مقاله
Preparation of Crack-free 3Y-TZP/AI2O3 Composite Ceramic Fiber by Electrolysis-sol-gel Method*
چکیده انگلیسی
Polycrystalline 3Y-TZP/Al2O3 tetragonal zirconia fiber was obtained by the pyrolysis of gel fibers using zirconium oxychloride octahydrate (ZOC) as the raw material. The spinnable zirconia sol was prepared by electrolyzing the zirconium oxychloride octahydrate (ZOC) solution in the presence of acetic acid and sugar (sucrose, glucrose or fructose), in which the molar ratios of CH3COOH/ZOC and sugar/ZOC were 1. 0-4. 0 and 0. 2-0. 4, respectively. The prepared tetragonal zirconia fibers sintered at different temperatures showed smooth and crack-free surfaces with diameters of 5-10 μm. The addition of Al2O3 enhanced the sintering process and prevented the crystals from growing. Thermogravimetric analysis (TG), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), and scanning electron microscope (SEM) techniques were used to characterize the prepared fibers.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Chemical Research in Chinese Universities - Volume 23, Issue 4, July 2007, Pages 377-380