Evolution of the intergranular phase during sintering of CaCu3Ti4O12 ceramics
چکیده انگلیسی

CaCu3Ti4O12 (CCTO) ceramics have been processed by solid state reaction and sintered at 1100 °C for different times. A clear increase of the dielectric constant of the material up to values of 6 × 104 has been observed with the sintering time. This increase is accompanied by a limited grain growth and intergranular Cu-oxide phase thickness reduction. The disappearance of the Cu-oxide phase is caused by the incorporation of Cu cations into the grains, contributing to the increase of the dielectric constant. Raman spectroscopy shows the decrease of TiO6 octahedral rotational modes with the sintering time due to the incorporation of Cu cations into the CCTO grains. XANES measurements show that the Cu main oxidation state is Cu2+ and does not change with the sintering time. The fitting of the experimental dielectric constant to the Internal Barrier Layer Capacitance (IBLC) model reveals the change of the intergranular phase dielectric constant, caused by a compositional change due to the incorporation of Cu into the CCTO grains.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of the European Ceramic Society - Volume 30, Issue 3, February 2010, Pages 737–742
نویسندگان
, , , , ,