کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1481186 | 1510458 | 2013 | 8 صفحه PDF | دانلود رایگان |

• Different methods to study the behaviors of metakaolin-based potassium geopolymer in HCl solution
• Geopolymer network intact after the acid attacks during 28 days
• High content of K species found in the solution after the acid attacks
This work studies the behavior of a metakaolin-based potassium geopolymer immersed in HCl solution (pH = 2). The polymer was attacked in three different ways to determine the effects of the immersion time, successive acid attack and the S/V value (sample mass/volume of solution) on the released elements and on pH. XRD, SEM and compressive strength studies showed that the basic geopolymer network remains intact regardless of the attack method. pH monitoring and FTIR demonstrated the existence of KHCO3 and K2CO3, likely resulting from the excessive KOH after the geopolymer samples react with atmospheric CO2. These basic species were considered the main products of the initial immersion in HCl solutions.
Journal: Journal of Non-Crystalline Solids - Volume 380, 15 November 2013, Pages 95–102