Fabrication of transparent plasma display can be demonstrated by simply applying the scatter-less nanophosphors to the currently available plasma display panel (PDP) scheme. For this goal, the optimization of the nanophosphors with respect to size and luminescence is necessary to produce a uniform, transparent, bright emissive layer. To develop red-emitting nanophosphors suitable for transparent PDP fabrication, we hydrothermally synthesized red-emitting Y(V,P)O4:Eu nanophosphors having various V/P ratios and Eu concentrations and varied their subsequent annealing condition. When Y0.94(V0.5,P0.5)O4:Eu0.06 nanophosphor annealed at 1000 °C for 1 h was used, 1.1 μm thick, uniform emissive layer with a high visible transmittance value of 72% was generated on glass substrate by a conventional screen-printing. Mini-sized test panels of transparent red-emitting plasma display were constructed by combining the rear plate (Y(V,P)O4:Eu nanophosphor layer/glass) and the front plate used in alternating current (ac)-type PDP structure, and their discharge luminance characteristics were evaluated.
► Hydrothermal synthesis of red Y(V,P)O4:Eu nanophosphors.
► Optimization of nanophosphor through control of composition and annealing.
► Transparent nanophosphor layer with a high visible transmittance value.
► Demonstration of transparent red-emitting plasma display device.
Journal: Materials Chemistry and Physics - Volume 135, Issue 1, 16 July 2012, Pages 51–57