Effect of heating conditions on pore structure and performance of carbon foams
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد شیمی مواد
پیش نمایش صفحه اول مقاله
Effect of heating conditions on pore structure and performance of carbon foams
چکیده انگلیسی
Carbon foams were prepared from AR pitch in a high pressure/high temperature reactor under different heating conditions. Their pore structure, bulk density, porosity, compressive strength, thermal conductivity, and crystallite size parameters were measured. Foams produced using a long time at a constant foaming temperature exhibit bigger pore size (412 nm), higher porosity (83.82%), lower bulk density (0.34 g/cm3), higher compressive strength (4.92 MPa), and more interconnected pores than that produced in a short time at the same constant foaming temperature, which exhibit high thermal conductivity (71.34 W/(m · K)) and low interlayer d-spacing (d002) (0.335 56 nm) after graphitization at 2800 °C. The specific thermal conductivity of graphite foams can reach 210 (W · (m · K)−1)/(g · cm−3), which is about five times greater than copper and four times greater than aluminum.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: New Carbon Materials - Volume 24, Issue 4, December 2009, Pages 321-326
نویسندگان
, , , ,