Performance of alloy 800H for high-temperature heat exchanger applications
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
دانش مواد (عمومی)
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
The tensile properties of austenitic Alloy 800H have been evaluated at temperatures ranging from ambient to 1000 °C. The results indicate that the tensile strength was gradually reduced with increasing temperature. Between ambient temperature and 200 °C, the failure strain was reduced possibly due to the occurrence of dynamic strain aging followed by its enhancement at temperatures up to 500 °C. Alloy 800H did not exhibit any failure in an acidic solution at constant-load. However, the true failure stress in this environment was reduced at elevated temperatures under a slow-strain-rate condition. The magnitude of electrochemical potentials became more active with increasing temperature. A detrimental effect of more noble controlled potential on the cracking susceptibility was noted in terms of the true failure stress. A combination of ductile and intergranular brittle failures was seen in the primary fracture surface of the tested cylindrical specimens.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: A - Volumes 452â453, 15 April 2007, Pages 665-672
Journal: Materials Science and Engineering: A - Volumes 452â453, 15 April 2007, Pages 665-672
نویسندگان
Ajit K. Roy, Vinay Virupaksha,