چکیده انگلیسی
The effect of glass additives on the densification and microwave dielectric properties of (Zr0.8, Sn0.2)TiO4 (ZST) ceramics were investigated. Three glasses including ZnO–B2O3–SiO2–Li2O–CuO (ZBSLC), BaO–B2O3–SiO2–Li2O–CuO (BBSLC) and BaO–SiO2–TiO2–CuO (BSTC) were selected for this study. Host material (Zr0.8, Sn0.2)TiO4 calcined at 1150 °C for 6 h was selected to be sintered with glasses in the temperature range of 950–1150 °C. For (Zr0.8, Sn0.2)TiO4 with 10 wt.% glass BBSLC sintered at 1050 °C, the ɛr of 30, Q × f value of 30300 and τf of −4 ppm/°C were obtained. Taking advantage of further milling to reduce the particle size, the ZST ceramics can be sintered at 1000 °C with ɛr = 26.8 and Q × f = 21900.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: A - Volume 426, Issues 1–2, 25 June 2006, Pages 143–146
Journal: Materials Science and Engineering: A - Volume 426, Issues 1–2, 25 June 2006, Pages 143–146
نویسندگان
Yuh-Ruey Wang, Sea-Fue Wang, Chung-Kai Wen,