کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1595133 1002764 2008 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
High temperature thermoelectric properties of Ca1−xBixMn1−yV yO3−δ (0≤x=y≤0.08)
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد دانش مواد (عمومی)
پیش نمایش صفحه اول مقاله
High temperature thermoelectric properties of Ca1−xBixMn1−yV yO3−δ (0≤x=y≤0.08)
چکیده انگلیسی

CaMnO3−δ with complex additives Bi2O3–V 2O5 were prepared by the solid-state reaction. The crystal structures of the Ca1−xBixMn1−yV yO3−δ (0≤x=y≤0.08) solid solutions were determined by means of the powder X-ray diffraction (XRD) using Rietan 2000 program and the high temperature thermoelectric properties were also investigated. Perovskite-type Ca1−xBixMn1−yV yO3−δ solid solutions are n-type semiconductors. The lattice parameters increase with increasing dopant level. The high temperature thermoelectric properties are improved due to Bi2O3–V 2O5 simultaneous doping. A maximum ZT value reaches to 0.21 for electron-doped Ca0.96Bi0.04Mn0.96V 0.04O3−δ at 1050 K, which is about twice as high as that of CaMnO3−δ. The thermal shock resistance at temperatures between 20 and 450 ∘C is also highly improved.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Solid State Communications - Volume 145, Issue 3, January 2008, Pages 132–136
نویسندگان
, , ,