Effect of withdrawal rate on microstructure and mechanical properties of a directionally solidified NiAl-based hypoeutectic alloy doped with trace Hf and Ho
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
Effect of withdrawal rate on microstructure and mechanical properties of a directionally solidified NiAl-based hypoeutectic alloy doped with trace Hf and Ho
چکیده انگلیسی

The hypoeutectic alloy, with nominal composition NiAl–31Cr–2.9Mo–0.1Hf–0.05Ho (at.%), was directionally solidified at three different withdrawal rates by liquid metal (Sn) cooling technique. Microstructural examination reveals that directional solidification gave rise to a shift in the coupled zone for the eutectic growth towards the Cr(Mo) phase. With the withdrawal rates increasing from 3 mm/min to 15 mm/min, the volume fraction of primary dendritic NiAl increases from 21.1% to 25.9%, while the size and the arm spacing of NiAl primary dendrite reduces simultaneously. The room temperature (RT) fracture toughness and the tensile strength at RT and elevated temperature (1373 K) present the valley value at intermediate rate (8 mm/min) among the withdrawal rate range which could be attributed to the decrease in volume fraction of eutectic NiAl/Cr(Mo) microstructure and the refinement of microstructure resulted from the increase of withdrawal rates. In terms of RT tensile elongation, the DS alloy grown at different withdrawal rates all break with no plastic flow.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Intermetallics - Volume 19, Issue 2, February 2011, Pages 206–211
نویسندگان
, , , , ,