عنوان انگلیسی مقاله ISI
Tungsten-vanadium-yttria alloys for fusion power reactors (I): Microstructural characterization
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
فلزات و آلیاژها
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
The densification in the compacts shows an increase with the V and Y2O3 additions. Porosity is reduced because of the formation of a W-V solid solution and V pools that fill the pores between the grains, although such effect is mainly observed in the W2V0.5Y alloy. The microstructure of pure W is composed of coarse polyhedral grains whereas a few coarse W grains, V pools and a nanostructured area, composed of fine W grains with dispersed Y, form the alloys. In contrast to previously studied W-4 wt.% V alloys, the V pools exhibit a reduction in the oxygen content, which prevents the formation of acicular oxide structures. Finally, the refinement of the microstructure induced by the addition of V and Y2O3 was analysed by electron backscattered diffraction measurements. Pure W presents high amount of grains over 1 μm (around 60% of the volume fraction) and only 2% below 100 nm. In the new alloys meanwhile, the population of micron size grains is highly reduced to less than 10% and grains smaller than 100 nm represent the 20%.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Refractory Metals and Hard Materials - Volume 54, January 2016, Pages 433-438
Journal: International Journal of Refractory Metals and Hard Materials - Volume 54, January 2016, Pages 433-438
نویسندگان
T. Palacios, M.A. Monge, J.Y. Pastor,