کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1604125 1516000 2010 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
W-15 wt%Cu nano-composite produced by hydrogen-reduction/sintering of WO3-CuO nano-powder
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
W-15 wt%Cu nano-composite produced by hydrogen-reduction/sintering of WO3-CuO nano-powder
چکیده انگلیسی
A two-stage hydrogen-reduction/sintering procedure was used to synthesize W-15 wt%Cu nano-composite tablets. Hydrogen-reduction was carried out at 600, 650, 700 and 750 °C for 15-90 min and sintering was performed at 1100, 1150, 1200 and 1250 °C for 60 min. Morphology and grain size of the products were rigorously investigated by scanning electron microscope (SEM), X-ray diffractometer (XRD) and nano-particle Zeta-sizer. Maximum consolidation of the nano-composite product was achieved at 1200 °C. Hydrogen-reduction at 700 °C for 90 min showed an average particle size of ∼72.9 nm. Total reduction was achieved at higher temperatures and longer times. The mixture had a homogeneous structure with 16.1 ± 0.1 g/cm3 density when sintered at 1200 °C for 60 min.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Refractory Metals and Hard Materials - Volume 28, Issue 3, May 2010, Pages 441-445
نویسندگان
, , ,