کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1629524 1006148 2011 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Hot Working Characteristics of Corrosion-Resistant Alloys G3 and 825
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
Hot Working Characteristics of Corrosion-Resistant Alloys G3 and 825
چکیده انگلیسی

The G3 and 825 alloys, with excellent combination of mechanical properties and corrosion resistance, can be used in hot, and acid environments. Thermal simulation tests were conducted on the alloys G3 and 825 in the THERMECMASTOR-Z simulator, at temperature between 1030 and 1300 °C, with strain rate from 1 to 50 s−1 and strain ɛ=0.8. The variations of flow stress with deformation temperature and strain rate were presented. Change of alloy structure with hot deformation and effect of strain rate on alloy dynamic recrystallization have been studied through microstructure observation by OM, SEM and TEM. Moreover, hot plasticity characteristics of alloy were analyzed by temperature-reduction of area curves. The results showed that available hot working temperature for G3, G3-Z and 825 was 1 100 to 1 240 °C, 1 130 to 1 220 °C and 1 050 to 1 240 °C, respectively. The reliable information on hot working in the alloy pilot production in steelwork is given.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Iron and Steel Research, International - Volume 18, Issue 4, April 2011, Pages 68-72