Microstructure and mechanical properties of Ti6Al4V powder compacts prepared by magnetic pulse compaction
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
Microstructure and mechanical properties of Ti6Al4V powder compacts prepared by magnetic pulse compaction
چکیده انگلیسی

Ti6Al4V powder compaction was performed by using magnetic pulse compaction in air at 200 °C. Effects of process parameters such as voltage, capacitance, discharge times on the microstructure, compressive strength, hardness and relative density of compacts were investigated. The experimental results show that the relative density, hardness and compressive strength of compacted specimens increase with increasing voltage. In addition, the relative density and compressive strength of compacted specimens increase with the augmentation of capacitance in the range investigated. The relative density increases, the hardness firstly increases and then tends to be a fixed value; and the compressive strength firstly increases and then decreases from one to five times compaction. Both values of the hardness and compressive strength reach the maxima of HRA 69.1 and 1 062.31 MPa, at three times compaction, respectively. There are pores in and between particles.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Transactions of Nonferrous Metals Society of China - Volume 20, Issue 4, April 2010, Pages 553-558