Crystal growth of tungsten during hydrogen reduction of tungsten oxide at high temperature
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
Crystal growth of tungsten during hydrogen reduction of tungsten oxide at high temperature
چکیده انگلیسی

Crystal growth of tungsten during hydrogen reduction of tungsten oxide (WO3) to prepare coarse grain tungsten powder at high temperature (950 °C) was studied. The phase composition and morphologies of products were investigated by means of XRD and SEM. The results show that the reduction sequence of hydrogen reduction of WO3 is WO3→WO2.9→W18O49→WO2→W. The step of WO2→W is the critical step which determines the grain size of tungsten powder. The partial pressure (pH2O/pH2) of H2O within powder layer shows strong effect on the nucleation and grain growth of tungsten. By increasing the pH2O/pH2within powder layer, well-developed coarse grain tungsten powder with particle size above 15 μm is obtained. After carburizing, the powder can be used to produce ultra-coarse grain cemented carbide with grain size above 5 μm.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Transactions of Nonferrous Metals Society of China - Volume 19, Supplement 3, December 2009, Pages s785-s789