The influences of sintering conditions on electrical properties of the 0.8Pb(Zr1/2Ti1/2)O3–0.2Pb(Co1/3Nb2/3)O3 ceramics have been investigated with sintering temperatures of 1175, 1200, 1225, and 1250 °C and dwell times for 2, 6, and 10 h. The crystal structure of dense specimens showed coexistence between tetragonal, rhombohedral and pseudo cubic phases in all sintering temperatures, while tetragonal-rich phase appeared with increasing dwell times. A maximum dielectric constant was observed at sintering condition of 1200 °C for 2 h, while the transition temperature slightly increased with increasing dwell time. All ceramics also showed diffused phase transition behaviors with a minimum diffusivity at sintering condition of 1200 °C for 2 h. In addition, the polarization–electric field (P–E) hysteresis loops of the ceramic systems also changed significantly with sintering conditions. Interestingly, the ferroelectric parameters; remnant polarization (Pr) and loop squareness (Rsq) tended to increase with increasing sintering temperatures and dwell times.
Journal: Current Applied Physics - Volume 9, Issue 5, September 2009, Pages 1165–1169