کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1800912 1024551 2010 10 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
The effects of annealing at 1000 °C for 24 h on the extrinsic properties of Pr–Fe–B and Nd–Fe–B-type sintered magnets
موضوعات مرتبط
مهندسی و علوم پایه فیزیک و نجوم فیزیک ماده چگال
پیش نمایش صفحه اول مقاله
The effects of annealing at 1000 °C for 24 h on the extrinsic properties of Pr–Fe–B and Nd–Fe–B-type sintered magnets
چکیده انگلیسی

Recent studies have shown the effects of a post sintering heat treatment at 1000 °C for 24 h on the microstructure and magnetic properties of Pr–Fe–B/Nd–Fe–B magnets based on Nd16Fe76B8 and Pr16Fe76B8. In an attempt to understand the influence of environmental factors, an investigation into the effects of annealing under different degrees of vacuum for both types of sintered magnets has been carried out. The effect of annealing the Pr–Fe–B magnets at 1000 °C for 24 h resulted in a general increase in the magnetic properties, especially the intrinsic coercivity, although the degree of improvement appeared to be dependent on the initial annealing conditions (ambient pressure). Oxygen analysis of sintered and annealed magnets indicates a change in the nature of the grain boundary phases after the annealing treatment. The effect of annealing the Nd–Fe–B magnets at 1000 °C for 24 h resulted in a general decrease in the magnetic properties, especially the intrinsic coercivity.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Magnetism and Magnetic Materials - Volume 322, Issue 1, January 2010, Pages 36–45
نویسندگان
, , ,