In this research, the oligomers were synthesized by the polycondensation of diamins (1,4-diamino-2-nitrobenzene and 2,5-diaminotoluene sulfate) with dialdehydes (terephtaldehyde 4,4′-diformylbiphenyl, bis(4-formylphenyl) ether and p-phenylene diacrolein). In this study, the oligoazomethines (OAMs) were studied using IR and UV–visible spectra and X-ray diffraction. The initial degradation temperatures (IDT) determined from TGA of OAMs were in the range of 225–270°C indicating their good thermal stability. The conductivity measurements of OAMs were carried out with an electrometer using four-point probe technique. The highest conductivity increase among all the oligoazomethine/char composites was observed for the OAMs composites formed with 30% char ratio.
The oligomers were synthesized by the polycondensation of diamins (1,4-diamino-2-nitrobenzene and 2,5-diaminotoluene sulfate) with dialdehydes (terephtaldehyde 4,41-diformylbiphenyl, bis(4-formylphenyl) ether and p-phenylene diacrolein).Figure optionsDownload as PowerPoint slide
Journal: Journal of Industrial and Engineering Chemistry - Volume 19, Issue 4, 25 July 2013, Pages 1340–1349