ObjectiveTo compare the long-term clinical effects of two kinds of crowns and bridges made of porcelain fused to Au-Pt alloy and Ni-Cr alloy.MethodsA total of 131 teeth (64 patients) were rehabilitated using porcelain-fused-to-metal crowns, among which 59 were rehabilitated with Au-Pt alloy metal ceramic crown and 72 with Ni-Cr alloy metal ceramic crown. The porcelain fracture, shade, marginal adaptation, gingival discoloration, and gingival status after finishing restoration and 36 months of follow-up were evaluated.ResultsAfter 36 months of restoration, porcelain fused to Au-Pt alloy crown showed better clinical effects than porcelain fused to Ni-Cr alloy crown in shade, marginal adaptation, gingival discoloration, as well as gingival status (all P<0.05).ConclusionThe Au-Pt alloy ceramic crown is superior to Ni-Cr alloy ceramic crown in long-term clinical effects.
Journal: Chinese Medical Sciences Journal - Volume 27, Issue 3, September 2012, Pages 167-170