High-lead flip chip bump cracking on the thin organic substrate in a module package
موضوعات مرتبط
مهندسی و علوم پایه مهندسی کامپیوتر سخت افزارها و معماری
پیش نمایش صفحه اول مقاله
High-lead flip chip bump cracking on the thin organic substrate in a module package
چکیده انگلیسی

Flip chip bump cracking was observed after Si die attach reflow on the organic substrate of a module package. High-lead bump and eutectic SnPb cladding were used on Si die and the substrate sides, respectively. The reflow peak temperature was 260 °C for compatibility with passive components attach using lead-free solder. Flip chip bump cracking occurred at high-lead solder close to the die side. The cracking was eliminated by lowering the reflow peak temperature down to 225 °C. Main cause of the cracking at 260 °C reflow was attributed to the extensive Sn diffusion into high lead bump. This decreased the melting point of the high-lead solder around the die side, which in turn worsened the adhesion between solder and die due to the coexistence of solid and liquid. Diffusion length estimation showed both of the liquid- and solid-state diffusions of Sn. Crack gap in the solder bump was consistent with thermal expansion mismatch between Si die and organic substrate. The bump cracking was mitigated by use of 225 °C reflow, limiting Sn diffusion and providing a good integrity of high lead bumps on die side.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Microelectronics Reliability - Volume 52, Issue 2, February 2012, Pages 455–460
نویسندگان
, , , , ,