کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
63335 47682 2007 10 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Study of Ir/WO3/ZrO2–SiO2 ring opening catalysts: Part I: Characterization
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی کاتالیزور
پیش نمایش صفحه اول مقاله
Study of Ir/WO3/ZrO2–SiO2 ring opening catalysts: Part I: Characterization
چکیده انگلیسی

This paper is the first part of a systematic study of the influence of W and Ir loading on the activity of Ir/WO3/ZrO2–SiO2 catalysts for the ring-opening reaction of naphthenic molecules using methylcyclohexane (MCH) as a model compound. A series of Si-stabilized tungstated zirconias, WOx/ZrO2–SiO2, containing up to 3.5 at W/nm2 was prepared. Ir-based catalysts containing up to 1.2 wt% were obtained by impregnation of these solids. The acidity of Si-stabilized tungstated zirconias, ZSiWx, was monitored by low-temperature CO adsorption followed by infrared (IR) spectroscopy. The results indicated the development of strong and relatively strong Brønsted acidity with increasing W surface density above a threshold of 1 atom W/nm2. The study of the Ir-doped solids showed that the texture, structure, and acidity of the ZSiWx solids were not affected by Ir deposition. The characterization of the metallic function was performed by hydrogenation of toluene and by CO adsorption at ambient temperature, followed by IR spectroscopy. Both methods indicated a low and constant Ir dispersion for the y  Ir/ZSiW0 (y=0.3y=0.3, 0.6, 1.2) series. For a given Ir loading (1.2Ir/ZSiWx), a progressive decrease in the dispersion of Ir metal with increasing W surface density was observed.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Catalysis - Volume 245, Issue 1, 1 January 2007, Pages 45–54
نویسندگان
, , , ,