Microstructure and mechanical properties of SiC joint with an in-situ formed SiC-TiB2 composite interlayer
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
دانش مواد (عمومی)
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
Diffusion bonding of SiC ceramic with in-situ formed SiC-TiB2 composite interlayer by reactive spark plasma sintering with B4C-Ti3SiC2-Si powder mixture was investigated. It was found that a dense composite interlayer between the SiC ceramic substrate could be obtained at 1600â¯Â°C for 10â¯min. Granular-shaped SiC with submicron-size and elongated TiB2 with micro-size were uniformly distributed in the bonding layer. The joint strength and hardness of the composite interlayer increased as the joining temperature increased up to 1600â¯Â°C due to the improved relative density and the higher fraction of elongated TiB2 phase. The grain growth and formation of micro-cracks deteriorated the mechanical strength of the 1700â¯Â°C joint. The maximum shear strength of 128.0â¯Â±â¯7.3â¯MPa was achieved for the joint bonded at 1600â¯Â°C. The toughening mechanisms of crack deflection, crack bridging and crack branching, and hardening mechanism of dual phase strengthening were observed in the morphology of indentation cracks.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: A - Volume 735, 26 September 2018, Pages 104-113
Journal: Materials Science and Engineering: A - Volume 735, 26 September 2018, Pages 104-113
نویسندگان
Zhiquan Wang, Huaxin Li, Zhihong Zhong, Ankang Yang, Yucheng Wu,