Sintering mechanisms of Al2O3-based composite ceramic tools having 25% Si3N4 additions
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
فلزات و آلیاژها
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
A type of Al2O3-based composite ceramic tool material simultaneously reinforced with about 25â¯wt% α-Si3N4 and β-Si3N4 grains was sintered using the vacuum hot-pressing technology by optimizing process parameters which included different contents of yttria additive, sintering temperature and time. Effects of these process parameters on densification, microstructure and mechanical properties were investigated. The mechanical properties of the composites increased and then decreased with an increase in the yttria content and sintering time. Low content of yttria led to a poor relative density and excess yttria caused inhomogeneous microstructure, which decreased the mechanical properties of the composites. The shorter sintering time led to the elongated β-Si3N4 grains stunted and porosity, and the longer sintering time led to β-Si3N4 grains coarsened and some agglomerations. The experimental results showed that the composite Al2O3/Si3N4 containing 1.5â¯wt% yttria, which was sintered under a pressure of 32â¯MPa at 1500â¯Â°C for 20â¯min, had the highest density and the optimal comprehensive mechanical properties. Its relative density, flexural strength, fracture toughness and hardness were 99.6â¯Â±â¯0.2%, 1093â¯Â±â¯32â¯MPa, 6.8â¯Â±â¯0.2â¯MPaâ¯m1/2, and 19.5â¯Â±â¯0.3â¯GPa respectively. The correlations between densification, mechanical properties and microstructure were discussed. The improvement of the mechanical properties was ascribed to equiaxed α-Si3N4 particles and elongated β-Si3N4 grains which induced the toughening and strengthening effects such as the crack deflection, interface debonding, grain fracture and grain pullout. The mixed fracture mode, high density, fine and homogenous microstructure, the stronger interface bonding and the pinning or bridging connection of the core-shell promoted the mechanical properties of the composite ceramic tool materials.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Refractory Metals and Hard Materials - Volume 73, June 2018, Pages 132-138
Journal: International Journal of Refractory Metals and Hard Materials - Volume 73, June 2018, Pages 132-138
نویسندگان
Xiaolan Bai, Chuanzhen Huang, Jun Wang, Bin Zou, Hanlian Liu,