کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
862103 | 1470799 | 2012 | 10 صفحه PDF | دانلود رایگان |

The onset resistivity transition temperature (Tc) is as high as 56.5K in the SmO0.7F0.3FeAs sample prepared by the two-step solid state reaction method. The Jc of the sample is 2.3×105A/cm2 (10K and 0T). The Tc of the fluorin over-doped SmO0.7F0.35FeAs and SmO0.7F0.4FeAs samples prepared by the two-step solid state reaction method at 1100°C for 20 hours are 56K and 55K, and the Jc are 1.9×105A/cm2 and 1.7×105A/cm2 (10K and 0T), respectively. The XRD results show that the lattice parameters a and c decrease systematically with increasing x between 0
Journal: Procedia Engineering - Volume 27, 2012, Pages 20-29