Relationships between microstructures and properties of buffer layer with Inconel 52M clad on AISI 316L stainless steel by GTAW processing
Keywords: نیکل فوق العاده ذوب شده; Mechanical characterization; Nickel based superalloys; Steel; Cladding; Welding; Failure;