In-vivo degradation mechanism of Ti-6Al-4V hip joints
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد بیومتریال
پیش نمایش صفحه اول مقاله
In-vivo degradation mechanism of Ti-6Al-4V hip joints
چکیده انگلیسی
The degradation mechanism was concluded to be of combined mechanical and chemical nature. Wear debris is formed and accumulated in large flakes (> 100 μm). Upon further sliding the flakes are pressed into the surface and ultimately crushed into small, brittle particulate debris (< 5 μm), which is released from the surface. It is suggested, that the small brittle particulate debris has a more detrimental effect in the hip joint than the large flakes due to a stronger reaction of the peri-prosthetic tissue. Also, Al-oxide particles are formed as part of the degradation mechanism.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: C - Volume 31, Issue 2, 12 March 2011, Pages 120-127
نویسندگان
, , ,