Improved ferroelectricity of (1−x)Na0.5Bi0.5TiO3-xBaTiO3 ceramics rapidly sintered at low temperature
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد سرامیک و کامپوزیت
پیش نمایش صفحه اول مقاله
Improved ferroelectricity of (1−x)Na0.5Bi0.5TiO3-xBaTiO3 ceramics rapidly sintered at low temperature
چکیده انگلیسی
High insulating (1−x)Na0.5Bi0.5TiO3-xBaTiO3 (x=0-0.08) ceramics were rapidly sintered at low temperature and then enhanced polarizations were observed. (1−x)Na0.5Bi0.5TiO3-xBaTiO3 nano-powders were prepared by the sol-gel method and then their ceramics were rapidly sintered at 920-1150 °C. According to the saturated ferroelectric hysteresis loops, the acquired saturated and remnant polarizations are ~48 μC/cm2 and ~40 μC/cm2 at x=0.03-0.08, and the coercive electric field decreases from ~70 kV/cm of pure Na0.5Bi0.5TiO3 to ~30 kV/cm at x=0.06-0.08. Furthermore, the piezoelectric d33 is 166.8 pC/N at x=0.06, where the morphotropic phase boundaries occur. These improved properties are achieved because the leakage current is reduced through compressing the loss of Na and Bi components during ceramics׳ preparation process.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Ceramics International - Volume 40, Issue 8, Part A, September 2014, Pages 11819-11824
نویسندگان
, , , , , ,