Bauxite residue (red mud) as a pulverised fuel ash substitute in the manufacture of lightweight aggregate
ترجمه فارسی عنوان
بقایای بوکسیت (گلدان قرمز) به عنوان سوخت جایگزین خاکستر پودر در تولید سنگین وزن
موضوعات مرتبط
مهندسی و علوم پایه مهندسی انرژی انرژی های تجدید پذیر، توسعه پایدار و محیط زیست
چکیده انگلیسی
This study looked at the potential of bauxite residue or red mud to be used in the manufacture of lightweight aggregate in replacement of pulverised fuel ash (PFA), commonly used as a way of recycling problematic wastes. The percentage replacements of red mud with PFA were as follows: 25, 31, 38, 44 and 50%. These were blended in a mix with waste excavated clay and sewage sludge - all from the Chongqing municipality in China. Lightweight pellets were produced using a Trefoil rotary kiln and were sintered to 1200 °C. Results showed that 44% bauxite residue replacement produced lightweight pellets with the highest compressive strength, highest density and largest water holding capacity. This would be expected in materials with a low level of silicates, which causes insufficient glass phase viscosity and therefore poor bloating during firing; producing an aggregate with a higher density but with open pores that allowed for larger water absorption. All ratios of red mud aggregates were significantly reduced in pH after firing to around pH 8, and this reduced the leachability of the aggregates to levels below those set by the European landfill directive (2003/33/EC).
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Cleaner Production - Volume 112, Part 1, 20 January 2016, Pages 401-408
نویسندگان
, , , , , ,