کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1430847 | 987211 | 2008 | 5 صفحه PDF | دانلود رایگان |
The surface structure and biomedical properties of NiTi shape memory alloy (SMA) samples after undergoing electropolishing and chemical polishing are determined and compared employing scanning electron microscopy, X-ray photoelectron spectroscopy, inductively-coupled plasma mass spectrometry, hemolysis analysis, blood platelet adhesion test, and MTT test. The results indicate that after chemical polishing, there is still a high Ni concentration on the surface of the NiTi SMA. On the other hand, electropolishing can form a thin surface titanium oxide film (about 10 nm thickness) with depleted Ni. In addition to the TiO2 phase, some titanium suboxides (TiO and Ti2O3) are found in the surface film. Compared to chemical polishing, electropolishing can more effectively mitigate out-diffusion of Ni ions and the wettability, blood compatibility, and thromboresistance are also better. However, no difference on the cytocompatibility can be observed from samples that have been chemically polished or electropolished.
Journal: Materials Science and Engineering: C - Volume 28, Issue 8, 1 December 2008, Pages 1430–1434