کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1441762 | 1509426 | 2011 | 11 صفحه PDF | دانلود رایگان |

The direct mixing of aqueous ferric chloride and o-phenylenediamine (OPD) solution at room temperature in the absence and presence of carbon nanotubes (CNTs) has been used to prepare poly(o-phenylenediamine) (POPD) micro-fibers and composites of the type CNTs/POPD having nanotubes incorporated in polymer fiber mass. Using surface enhanced infrared absorption (SEIRA) spectroscopy significant modifications in the low frequency range of the polymer spectrum are revealed when Au is used as metallic support. Similar variations are reported for the POPD samples prepared by the electropolymerization of OPD onto rough Au electrode. A covalent functionalization of CNTs with POPD and a doping process of POPD with radical anions of CNTs is proved by surface enhanced resonant Raman scattering and SEIRA spectroscopy. The X-ray diffraction (XRD) studies indicate a high crystallinity both for POPD and CNTs/POPD composites prepared by chemical or electrochemical methods.
Figure optionsDownload as PowerPoint slideHighlights
► One-dimensional composites based on SWCNTs and POPD are synthesized.
► SEM studies show an incorporation of SWCNTs in POPD fibers mass.
► The adsorption of POPD and SWNTs on Au support are investigated by SEIRA spectroscopy.
► Using SERS spectroscopy a functionalization of SWCNTs with POPD is demonstrated.
Journal: Synthetic Metals - Volume 161, Issues 21–22, November–December 2011, Pages 2344–2354