چکیده انگلیسی

Zirconium titanate powders were synthesized by a straightforward sol–gel method using zirconium and titanium chlorides as metal precursors, deionized water as solvent and oxygen donor, and a NaOH solution for adjusting pH to 7. According to transmission electron microscopy, amorphous particles of nearly 5 nm in size with a relatively spherical morphology were prepared. Thermogravimetry and differential scanning calorimetery analyses on the xerogel at a heating rate of 10 °C/min indicated a crystallization temperature of 690 °C, which is comparable with previous reports. Furthermore, via differential scanning calorimetery studies using the Kissinger's equation, the activation energy for ZrTiO4 crystallization was determined to be 850 kJ/mol. Structural evaluations in the isothermal regime, using X-ray diffraction experiments, implied the onset of ZrTiO4 crystallization at 550 °C.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Ceramics International - Volume 38, Issue 8, December 2012, Pages 6145–6149
نویسندگان
, , , , , ,