Fabrication of laminated SiCw/SiC ceramic composites by CVI
چکیده انگلیسی

Laminated SiCw/SiC ceramic composites were prepared by chemical vapor infiltration (CVI) and tape casting, and the advantages of this method were investigated. The results showed that this method can increase strength of the composites by reducing the damage of SiC whiskers and increasing their volume fraction, and increase toughness of the composites by controlling the interfacial bonding between whiskers and matrix and inter-laminar bonding between layers. The volume fraction of whiskers reached 40 vol.%, and the flexural strength, tensile strength and fracture toughness were 315 MPa, 158 MPa and 8.02 MPa m1/2, respectively. Interfacial and interlaminar crack deflection and bridging were observed.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of the European Ceramic Society - Volume 33, Issue 10, September 2013, Pages 1701–1706
نویسندگان
, , , , ,