The study of molecular dynamics by broadband dielectric spectroscopy (BDS) is presented for polyurethane (PU), poly(2-hydroxyethyl methacrylate) (PHEMA) and for semi-IPNs based on PU and PHEMA synthesized by photopolymerization. The dielectric properties were performed in wide range of frequencies and temperatures with the goal to establish the relation between the relaxations and the structure. Five relaxation phenomena were finally detected for PHEMA : γ-, βsw-, β-relaxations at low temperatures and α-relaxation at 150 °C at high frequencies plus ionic conductivity relaxation which starts at 0 °C. For semi-IPNs the overlapping of γ- and βsw-relaxations of PHEMA (−125/−75 °C), then with increasing the temperature α-relaxation in PU (−75/0 °C), next ionic conductivity relaxation which starts at 0 °C, and finally the α-relaxation of PHEMA (+125/+170 °C) were detected. The α-relaxation of PHEMA in semi-IPNs shifts to lower temperatures and became broader with increasing amount of PU due to incomplete phase separation in the system and formation of interphases. The dielectric relaxation phenomena were fitted with Havriliak–Negami equation. Activation energy, τo and α parameters were calculated. For α-relaxations corresponding dielectric characteristics have been determined from Vogel–Fulcher–Tammann equation. The relaxation map for investigated PU, PHEMA and semi-IPNs was built.
Journal: Journal of Non-Crystalline Solids - Volume 355, Issues 28–30, 15 August 2009, Pages 1453–1460