Synthesis of cadmium selenide thin films by CBD method has been presented. The deposited film samples were subjected to XRD, SEM, UV-vis-NIR and TEP characterization. X-ray diffraction analysis showed that CdSe film sample crystallized in zinc blende or cubic phase structure. SEM studies reveal that the grains are spherical in shape and uniformly distributed all over the surface of the substrates. The optical band gap energy of as deposited film sample was found to be in the order of 1.8 eV. The electrical conductivity of the film sample was found to be 10−6 (Ω cm)−1 with n-type of conduction mechanism.
Figure optionsDownload as PowerPoint slideHighlights
► CdSe thin films deposited first time using formic acid as a complexing agent.
► The deposited thin films were characterized by XRD, SEM, UV-vis-NIR and electrical techniques.
► X-ray diffraction analysis shows presence of zinc blende crystal structure.
Journal: Materials Research Bulletin - Volume 46, Issue 10, October 2011, Pages 1600–1603