This study investigates the synthesis of single-phase nanocrystalline forsterite powder by mechanical activation with subsequent annealing. To produce forsterite powder, a mixture of talc and magnesium oxide powders was first milled by a planetary ball mill, and then annealed at 1000 and 1200 °C for 1 h. The synthesized powder was characterized by X-ray diffraction (XRD), simultaneous thermal analysis (STA), scanning electron microscopy (SEM), and atomic absorption spectrometry (AAS). The initial temperature of forsterite crystallization was reduced to about 825 °C after 20 h of mechanical activation. The forsterite powder synthesized by 5 h of mechanical activation with subsequent annealing at 1000 °C for 1 h had crystallites 40 nm in size. The particle size of this sample was less than 500 nm.
Journal: Materials Research Bulletin - Volume 45, Issue 4, April 2010, Pages 388–391